Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.19 W/m-K | 15.2 BTU-in/hr-ft²-°F | |
Resinlab® SEC1244 Silver Filled Epoxy Adhesive Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth.. |