Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 28.09 W/m-K @Temperature 540 °C |
194.9 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel CPM® 1V® High Alloy Tool Steel CPM 1V is a medium carbon, high alloy tool steel which exhibits high toughness combined with high heat resistance. It is suited for both hot or cold applications which demand high impact toughness a.. |