Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.34 - 2.87 W/m-K @Temperature 1450 °C |
9.30 - 19.9 BTU-in/hr-ft²-°F @Temperature 2640 °F |
Varies directly with relative density (8-16%) |
ERG Aerospace Duocel® Silicon Carbide Foam Silicon Carbide (SiC) foam is a porous, open-celled structure made from an interconnected lattice of ceramic ligaments. The pattern of cells and ligaments repeats regularly throughout the entirety o.. |