Thermal Properties Metric English Comments
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K

@Temperature 800 °C
181 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 26.1 W/m-K
181 BTU-in/hr-ft²-°F
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
Thermal Conductivity 26.1 W/m-K
181 BTU-in/hr-ft²-°F
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
Thermal Conductivity 26.1 W/m-K
181 BTU-in/hr-ft²-°F
Eagle Brass 430 Ferritic Stainless Steel, Annealed
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
Thermal Conductivity 26.1 W/m-K
181 BTU-in/hr-ft²-°F
Eagle Brass 430 Ferritic Stainless Steel, Full Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..