Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 288°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 316°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 482°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Thermal Conductivity | 24.899 W/m-K @Temperature 100 °C |
172.80 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |