Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, 1/2 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, 1/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, 3/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, Annealed CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, Extra Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, Extra Spring CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Thermal Conductivity | 159.1 W/m-K | 1104 BTU-in/hr-ft²-°F | |
Eagle Brass 230 Red Brass, Spring CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |