Polymer Property : Thermal Conductivity = 1104 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, 1/2 Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, 1/4 Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, 3/4 Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, Annealed
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, Extra Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, Extra Spring
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Thermal Conductivity 159.1 W/m-K
1104 BTU-in/hr-ft²-°F
Eagle Brass 230 Red Brass, Spring
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..