Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.16 W/m-K | 15.0 BTU-in/hr-ft²-°F | |
Cotronics Resbond™ 908 High Temperature Ceramic Adhesive, Moisture Proof |
|||
Thermal Conductivity | 2.16 W/m-K | 15.0 BTU-in/hr-ft²-°F | |
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose |
|||
Thermal Conductivity | 2.16 W/m-K @Temperature 93.3 °C |
15.0 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
Thermal Conductivity | 2.16 W/m-K | 15.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 122 500°F (260°C) Nickel Filled Adhesive and Casting Epoxy Specially formulated to provide an economical alternative to silver filled electrically conductive epoxies. Applications: for use in applications where highest electrically conductivity not required.. |
|||
Thermal Conductivity | 2.16 W/m-K | 15.0 BTU-in/hr-ft²-°F | |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |
|||
Thermal Conductivity | 2.16 W/m-K | 15.0 BTU-in/hr-ft²-°F | |
Aremco AREMCOLOX™ 502-676 Machinable Magnesium Oxide Full-fired, fine grain, high purity MgO ceramic. Inert to molten metals, slags, superconductors. Broad line of standard crucibles. Custom parts made to print. |