Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 139 W/m-K | 962 BTU-in/hr-ft²-°F | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |