Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 13.2 W/m-K | 91.6 BTU-in/hr-ft²-°F | |
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 13.2 W/m-K | 91.6 BTU-in/hr-ft²-°F | |
California Fine Wire Stablohm 675 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |