Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.87 W/m-K | 13.0 BTU-in/hr-ft²-°F | |
Cotronics Duralco™ 4525 Electrically Resistant, Room Temperature Curing Epoxy High bond strength, high thermal stability, low moisture absorption, low shrinkage and excellent chemical, electrical, and radiation resistance.Chemical Resistance: resistant to hydrochloric, phosph.. |
|||
Thermal Conductivity | 1.88 W/m-K | 13.0 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® ED1020 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Its unique features include exce.. |
|||
Thermal Conductivity | 1.87 W/m-K | 13.0 BTU-in/hr-ft²-°F | |
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose |