Thermal Properties Metric English Comments
Thermal Conductivity 12.6 W/m-K
87.4 BTU-in/hr-ft²-°F
RT
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Thermal Conductivity 12.6 W/m-K
87.4 BTU-in/hr-ft²-°F
RT
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i..
Thermal Conductivity 12.6 W/m-K

@Temperature 100 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes HR-120® alloy, solution heat-treated plate
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 12.6 W/m-K
87.4 BTU-in/hr-ft²-°F
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy
UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm..