Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.64 W/m-K | 11.4 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Thermal Conductivity | 1.64 W/m-K @Temperature 100 °C |
11.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Mateck Zero Expansion Glass - ZERODUR Optical crystals |