Thermal Properties Metric English Comments
Thermal Conductivity 1.64 W/m-K
11.4 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Thermal Conductivity 1.64 W/m-K

@Temperature 100 °C
11.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Mateck Zero Expansion Glass - ZERODUR
Optical crystals
Copyright © lookpolymers.com All Rights Reserved