Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 153 W/m-K | 1060 BTU-in/hr-ft²-°F | |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Thermal Conductivity | 153 W/m-K | 1060 BTU-in/hr-ft²-°F | |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Thermal Conductivity | 153 W/m-K | 1060 BTU-in/hr-ft²-°F | |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |