Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 104 W/m-K | 720 BTU-in/hr-ft²-°F | |
Materion moldMAX® HH High Hardness Beryllium Copper Alloy Description: moldMAX® and PROtherm® are Brush Wellman's copper beryllium alloys specifically designed for the plastic processing industry. These alloys provide a combination of thermal con.. |
|||
Thermal Conductivity | 104 W/m-K | 720 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |
|||
Thermal Conductivity | 104 W/m-K | 720 BTU-in/hr-ft²-°F | |
Cadi 40 MOLD-MOR™ A Beryllium Copper Alloy with moderate thermal conductivity and very high hardness.Information provided by Cadi Company. |