Polymer Property : Thermal Conductivity = 10.8 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.55 W/m-K
10.8 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy
A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding...
Thermal Conductivity 1.56 W/m-K
10.8 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr..