Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.256 W/m-K @Temperature 500 °C |
1.78 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Thermal Conductivity | <= 0.256 W/m-K @Temperature 500 °C |
<= 1.78 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Sharadaa Ceramics REFINSUL ZAP-016 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Thermal Conductivity | 0.257 W/m-K @Temperature 100 °C |
1.78 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1225 |
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |