Material Notes:
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for low density and low thermal conductivity, and are helpful in conserving heat energy thus reducing fuel costs.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density <= 1.10 g/cc
<= 0.0397 lb/in³
Dried at 110°C
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00118 GPa
0.171 ksi
Dried at 110°C
0.000490 GPa

@Treatment Temp. 1100 °C
0.0711 ksi

@Treatment Temp. 2010 °F
0.000588 GPa

@Treatment Temp. 800 °C
0.0853 ksi

@Treatment Temp. 1470 °F
Compressive Strength 1.18 MPa
171 psi
Fired at Service temp. of 1100°C, Cold Crushing
1.47 MPa
213 psi
Fired at 800°C, Cold Crushing
1.96 MPa
284 psi
Dried at 110°C, Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity <= 0.256 W/m-K

@Temperature 500 °C
<= 1.78 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Al2O3 >= 32 %
>= 32 %
Fe2O3 <= 6.0 %
<= 6.0 %
Descriptive Properties Value Comments
Permanent Linear Change -0.8 - 0.8%
Fired at 800°C
-1.2 - 1.2%
Fired at Service temp. 1100°C