Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.370 - 1.70 W/m-K | 2.57 - 11.8 BTU-in/hr-ft²-°F | Average value: 0.657 W/m-K Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |