Polymer Property : Thermal Conductivity = 1.51 BTU-in/hr-ft²-°F
Polymer Property :
Thermal Conductivity =
1.51 BTU-in/hr-ft²-°F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.218
W/m-K
1.51
BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Semitron® ESd 420- CM Dissipative Polyetherimide(ASTM Product Data Sheet)