Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.173 - 0.214 W/m-K | 1.20 - 1.49 BTU-in/hr-ft²-°F | Average value: 0.187 W/m-K Grade Count:12 |