Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.173 - 14.0 W/m-K | 1.20 - 97.2 BTU-in/hr-ft²-°F | Average value: 3.31 W/m-K Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Thermal Conductivity | 0.173 - 0.200 W/m-K | 1.20 - 1.39 BTU-in/hr-ft²-°F | Average value: 0.187 W/m-K Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | |
Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1804 Polycarbonate MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1837* Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1899* Polycarbonate, Impact Grade Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2865 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt tempe.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3158 Polycarbonate Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 3206 Polycarbonate ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® AG2677 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transparent colors on.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® Rx1805 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1243 Polycarbonate ISO 7391-PC,ELS,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityBranchedUV stabilizedEasy releaseAvailable in color code 550111onlyMulti wall sheet/profilesPreprocessi.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1260 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-24-9Global gradeMVR (300 °C/1.2 kg) 34 cm3/10 minImpact modifiedLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in light colors onlyPreproc.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LQ3187 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® KU1-1230* Polycarbonate ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Thermal Conductivity | 0.173 W/m-K | 1.20 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® LQ2687 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t.. |