Thermal Properties Metric English Comments
Thermal Conductivity 0.213 W/m-K
1.48 BTU-in/hr-ft²-°F
ASTM C177
Westlake Plastics Ardel® Polyarylate
Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res..