Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.213 W/m-K | 1.48 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Ardel® Polyarylate Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res.. |