Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.260 - 0.988 W/m-K | 1.80 - 6.86 BTU-in/hr-ft²-°F | Average value: 0.527 W/m-K Grade Count:11 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |