Thermal Properties Metric English Comments
Thermal Conductivity 0.350 - 0.965 W/m-K
2.43 - 6.69 BTU-in/hr-ft²-°F
Average value: 0.717 W/m-K Grade Count:8
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..