Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | ASTM C518-98 |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
Pyrotek TS-550 Insulating Board TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the form.. |
|||
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
Momentive Performance Materials TSE3941 Flame Retardant Adhesive Sealant, White TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
Schott N-SK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
Schott N-LAF21 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
Schott N-LAF7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
Dow Corning SE 4440 LP KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, low viscosity.Information provided by Dow Corning |