Thermal Conductivity 0.116 W/m-K

@Temperature 500 °C
0.805 BTU-in/hr-ft²-°F

@Temperature 932 °F
Pyrotek Pyromoldable JDR1150A Moldable Paste Type Low Density Refractory
ApplicationsLaunder linings Lining of distribution launders for DC casting table Industrial furnace linings Back up material behind hot face lining AdvantagesLow density with high insulating propert..