Polymer Property : Thermal Conductivity = 0.732 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.732 W/m-K
5.07 BTU-in/hr-ft²-°F
ASTM C177
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Thermal Conductivity 0.732 W/m-K
5.07 BTU-in/hr-ft²-°F
ASTM C177
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.