Thermal Properties Metric English Comments
Thermal Conductivity 0.730 W/m-K
5.07 BTU-in/hr-ft²-°F
Schott N-PK52A Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.732 W/m-K
5.07 BTU-in/hr-ft²-°F
ASTM C177
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Thermal Conductivity 0.732 W/m-K
5.07 BTU-in/hr-ft²-°F
ASTM C177
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Thermal Conductivity 0.730 W/m-K
5.07 BTU-in/hr-ft²-°F
Tra-Con Tra-Bond 224-8 Room Temperature Cure Epoxy Adhesive
TRA-BOND 224-8 room temperature cure epoxy adhesive is a thermally conductive version of 224-1. This adhesive develops structural strength rapidly. When cured at room temperature, this adhesive prov..
Thermal Conductivity 0.730 W/m-K

@Temperature 100 °C
5.07 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 1510 Polyester, Granular, Transfer Molded
PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file ..