Polymer Property : Thermal Conductivity = 0.625 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
ASTM C158
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam
Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products..
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
ASTM C518-98
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
Pyrotek F-24 Dense Machinable Board
F-24 is a high temperature resin material that is reinforced with fiberglass. Abrasion resistant, it is used for hot glass handling applications.ApplicationsDonut rollers for glass Guide rails Wear..
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
Pyrotek F-51 Dense Machinable Board
F-51 is a high temperature resin base, supplemented with fiberglass and graphite to provide extra strength and lubricity. F-51 is abrasion resistant and suitable for hot glass handling applications..
Thermal Conductivity 0.0900 W/m-K
0.625 BTU-in/hr-ft²-°F
ASTM C158
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..