Thermal Conductivity 0.300 - 0.562 W/m-K
2.08 - 3.90 BTU-in/hr-ft²-°F
Average value: 0.467 W/m-K Grade Count:10
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..