Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.5577 W/m-K | 3.864 BTU-in/hr-ft²-°F | ASTM C177 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Thermal Conductivity | 0.5577 W/m-K | 3.864 BTU-in/hr-ft²-°F | ASTM C177 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |