Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.418 - 0.460 W/m-K | 2.90 - 3.19 BTU-in/hr-ft²-°F | |
Polikim EFALON® C-25 PTFE, 25% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Thermal Conductivity | 0.370 - 0.460 W/m-K @Temperature 100 - 100 °C |
2.57 - 3.19 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.400 W/m-K Grade Count:4 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |