Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0519 W/m-K | 0.360 BTU-in/hr-ft²-°F | |
Mo-Sci Corporation GL-0193 Hollow Glass Spheres Appearance: Hollow microspheres with white color in powder form.Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu.. |