Thermal Properties Metric English Comments
Thermal Conductivity 0.0500 W/m-K
0.347 BTU-in/hr-ft²-°F
mean temp of 10°C; ISO 8302 1991
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Thermal Conductivity 0.0500 W/m-K
0.347 BTU-in/hr-ft²-°F
DIN 52 612
Brandenburger ISOFLEX AFV Foam
This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio..