Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0500 W/m-K | 0.347 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0500 W/m-K | 0.347 BTU-in/hr-ft²-°F | DIN 52 612 |
Brandenburger ISOFLEX AFV Foam This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio.. |