Thermal Properties Metric English Comments
Thermal Conductivity 0.0360 - 0.0432 W/m-K
0.250 - 0.300 BTU-in/hr-ft²-°F
Average value: 0.0399 W/m-K Grade Count:3
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..