Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam AIREX® C51 is a closed-cell polymer foam with outstanding damage tolerance and formability. Its excellent price / performance ratio uniquely qualifies this core material for high-volume sandwich .. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | 25g/L; KS M 3808 |
LG Chemical B160 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | 25g/L; KS M 3808 |
LG Chemical B240 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | 20g/L; KS M 3808 |
LG Chemical R120 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | 25g/L; KS M 3808 |
LG Chemical R320 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | ASTM-C-518 |
Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam Description: Closed cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side. The high-tack positioning adhesive grips tight on initial contact and keeps foam in place durin.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | mean temp of 0°C; ISO 8301 |
Zotefoams ZOTEK® N B50 High Performance Nylon Foam Zotek® N B50 is a closed cell, cross-linked polyamide-6 foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | Moisture Content: 5% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K @Temperature 40.0 °C |
0.250 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | |
3M 4052 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | |
3M 4056 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | |
3M 4085 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | Moisture Content: 5% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K @Temperature 40.0 °C |
0.250 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | Moisture Content: 5% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K @Thickness 50.0 mm, Temperature 40.0 °C |
0.250 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature 104 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | Moisture Content: 5% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K @Temperature 40.0 °C |
0.250 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | Moisture Content: 5% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K @Temperature 40.0 °C |
0.250 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | Moisture Content: 5% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K @Temperature 40.0 °C |
0.250 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | 16 g/l; EN 12667 |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |
|||
Thermal Conductivity | 0.0360 W/m-K | 0.250 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |