Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.241 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of.. |
|||
Thermal Conductivity | 0.241 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Thermal Conductivity | 0.241 W/m-K | 1.67 BTU-in/hr-ft²-°F | |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |