Polymer Property : Thermal Conductivity = 0.229 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
Zotefoams ZOTEK® F OSU Flexible PVDF Foam
Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and ..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
Zotefoams ZOTEK® F 30 PVDF Foam
Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
Zotefoams ZOTEK® F 35 PVDF Foam
Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Thermal Conductivity 0.0330 - 0.0500 W/m-K
0.229 - 0.347 BTU-in/hr-ft²-°F
ERG Aerospace Reticulated Vitreous Carbon (RVC)
Glass-like Carbon Foam
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F

@Temperature 50.0 °F
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in
DIN EN 13164
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F

@Temperature 50.0 °F
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in
DIN EN 13164
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in
DIN EN 13164
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm,
Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in,
Temperature 50.0 °F
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F

@Temperature 50.0 °F
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in
DIN EN 13164
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F

@Temperature 50.0 °F
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in
DIN EN 13164
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
Moisture Content: 0%
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Temperature 10.0 °C
0.229 BTU-in/hr-ft²-°F

@Temperature 50.0 °F
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K

@Thickness 50.0 mm
0.229 BTU-in/hr-ft²-°F

@Thickness 1.97 in
DIN EN 13164
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..