Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | mean temp of 0°C; ISO 8301 |
Zotefoams ZOTEK® F OSU Flexible PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | mean temp of 0°C; ISO 8301 |
Zotefoams ZOTEK® F 30 PVDF Foam Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | mean temp of 0°C; ISO 8301 |
Zotefoams ZOTEK® F 35 PVDF Foam Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0330 - 0.0500 W/m-K | 0.229 - 0.347 BTU-in/hr-ft²-°F | |
ERG Aerospace Reticulated Vitreous Carbon (RVC) Glass-like Carbon Foam |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | Moisture Content: 0% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Temperature 10.0 °C |
0.229 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in |
DIN EN 13164 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | Moisture Content: 0% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Temperature 10.0 °C |
0.229 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in |
DIN EN 13164 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | Moisture Content: 0% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in |
DIN EN 13164 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm, Temperature 10.0 °C |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature 50.0 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | Moisture Content: 0% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Temperature 10.0 °C |
0.229 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in |
DIN EN 13164 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | Moisture Content: 0% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Temperature 10.0 °C |
0.229 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in |
DIN EN 13164 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | Moisture Content: 0% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Temperature 10.0 °C |
0.229 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K @Thickness 50.0 mm |
0.229 BTU-in/hr-ft²-°F @Thickness 1.97 in |
DIN EN 13164 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0330 W/m-K | 0.229 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |