Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.173 - 0.202 W/m-K | 1.20 - 1.40 BTU-in/hr-ft²-°F | Average value: 0.180 W/m-K Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |