Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.159 - 0.187 W/m-K | 1.10 - 1.30 BTU-in/hr-ft²-°F | Average value: 0.180 W/m-K Grade Count:4 |