Thermal Properties Metric English Comments
Thermal Conductivity 0.0240 - 0.0370 W/m-K

@Temperature -80.0 - 50.0 °C
0.167 - 0.257 BTU-in/hr-ft²-°F

@Temperature -112 - 122 °F
Average value: 0.0312 W/m-K Grade Count:5
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Thermal Conductivity 0.0240 - 0.0370 W/m-K

@Temperature -80.0 - 50.0 °C
0.167 - 0.257 BTU-in/hr-ft²-°F

@Temperature -112 - 122 °F
Average value: 0.0312 W/m-K Grade Count:1
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Thermal Conductivity 0.0240 - 0.0370 W/m-K

@Thickness 50.0 - 50.0 mm
0.167 - 0.257 BTU-in/hr-ft²-°F

@Thickness 1.97 - 1.97 in
Average value: 0.0312 W/m-K Grade Count:1
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Thermal Conductivity 0.0240 W/m-K

@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F

@Temperature -112 °F
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0240 W/m-K

@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F

@Temperature -112 °F
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0240 W/m-K

@Thickness 50.0 mm,
Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F

@Thickness 1.97 in,
Temperature -112 °F
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0240 - 0.0370 W/m-K

@Temperature -80.0 - 50.0 °C
0.167 - 0.257 BTU-in/hr-ft²-°F

@Temperature -112 - 122 °F
Average value: 0.0312 W/m-K Grade Count:5
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Thermal Conductivity 0.0240 - 0.0370 W/m-K

@Temperature -80.0 - 50.0 °C
0.167 - 0.257 BTU-in/hr-ft²-°F

@Temperature -112 - 122 °F
Average value: 0.0312 W/m-K Grade Count:1
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Thermal Conductivity 0.0240 - 0.0370 W/m-K

@Thickness 50.0 - 50.0 mm
0.167 - 0.257 BTU-in/hr-ft²-°F

@Thickness 1.97 - 1.97 in
Average value: 0.0312 W/m-K Grade Count:1
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Thermal Conductivity 0.0240 W/m-K

@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F

@Temperature -112 °F
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0240 W/m-K

@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F

@Temperature -112 °F
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0240 W/m-K

@Temperature -80.0 °C
0.167 BTU-in/hr-ft²-°F

@Temperature -112 °F
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..