Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:5 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Thickness 50.0 - 50.0 mm |
0.167 - 0.257 BTU-in/hr-ft²-°F @Thickness 1.97 - 1.97 in |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Thermal Conductivity | 0.0240 W/m-K @Temperature -80.0 °C |
0.167 BTU-in/hr-ft²-°F @Temperature -112 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0240 W/m-K @Temperature -80.0 °C |
0.167 BTU-in/hr-ft²-°F @Temperature -112 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0240 W/m-K @Thickness 50.0 mm, Temperature -80.0 °C |
0.167 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature -112 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:5 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Temperature -80.0 - 50.0 °C |
0.167 - 0.257 BTU-in/hr-ft²-°F @Temperature -112 - 122 °F |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.0240 - 0.0370 W/m-K @Thickness 50.0 - 50.0 mm |
0.167 - 0.257 BTU-in/hr-ft²-°F @Thickness 1.97 - 1.97 in |
Average value: 0.0312 W/m-K Grade Count:1 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.0240 W/m-K @Temperature -80.0 °C |
0.167 BTU-in/hr-ft²-°F @Temperature -112 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0240 W/m-K @Temperature -80.0 °C |
0.167 BTU-in/hr-ft²-°F @Temperature -112 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0240 W/m-K @Temperature -80.0 °C |
0.167 BTU-in/hr-ft²-°F @Temperature -112 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |