Polymer Property : Thermal Conductivity = 0.162 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.162 W/m-K
1.12 BTU-in/hr-ft²-°F
DIN 52612
Polycasa COPOL PETG
QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v..