Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.105 W/m-K | 0.729 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 0.105 W/m-K @Temperature 300 °C |
0.729 BTU-in/hr-ft²-°F @Temperature 572 °F |
DIN 52612 |
Brandenburger ISOFLEX AFV Foam This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio.. |