Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0404 W/m-K | 0.280 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |